For use in the homokinetic ball joint of an automobile propeller shaft. Punched part made of 2.5 mm thick cementation steel. 
– Surface tolerance of the lower side Ra 0.8 µ.
– Tolerance of the underside towards the middle of    the dome-shaped cupola 0.02 mm. 
– Hardened and tempered to 700 HV.

Area of application

Weight

Automotive industry

92 g

Material

Material number

Cold-rolled steel strip  for thermal treatment 16MNCr5M

similar to 1.7131

Internnal processing

External processing

Deep drawing

Thermal treatment:

Stamping

Hardened and tempered to 700 +100 HV1

Forming

Testing